OneQuickGT1 said:what are your favorites? Looking for suggestions for some VW's and Audis I will be doing. I have the megs combo but looking for some others to use on the GG6.
Thanks!
thomasdekany said:Use wool or MF pads to start with, no matter what products you use. Naturally 105/UNO/101 (if you can get it) will do the best job as they are the most aggressive.
OneQuickGT1 said:Accumulator...do you then finish with a MF polishing pad and something like 205?
OneQuickGT1 said:Great...thanks!
Bill D said:I've always used PO85RD on any micromarring on Audi clear and Mercedes Ceramiclear.
Alfisti said:On a recent detail I found PowerGloss worked better than M105 and UNO4. Go figure. :nixweiss
Accumulator said:My "good" painter says the same thing! He swears his PG cuts a lot better than M105, did direct comparisons.
He was so unimpressed with M105 (sample of v1.0 from his Meg's rep) that he gave it to his wife to use on some householdy thing, maybe a cast-iron stove or somesuch.