I have a small harline scratch that you can't even feel with your fingernail. How long should I work SSR2 over it? Like is there such thing as working it TOO long? I have a PC and Megs pads. What color pad would you recommend aswell?
 
use the yellow polishing pad and work it until it is dry and almost gone, then wipe off the remaining residue with a mf towel - pc should be set @ 5-5.5
 
If you've used SSR2 before, you probably wouldn't worry about it not coming out if it's that light. It really works!
MY FIRST EXPERIENCE WITH IT:
I just got it and tried it on my winter swirled car (black, of course). I went with a white pad on the PC and it got rid of pretty much all swirls/scratches that weren't to the metal! And with only one pass! (well, a few passes, one application).
Later, when I was cleaning up, I realized I had used an Edge pad.
"So what?" you may ask.
So....Edge white pads are their "ultra fine finishing" pad! Not even a polishing pad!
Therefore, if SSR2 works this well with a finishing pad, imagine what a polishing pad can do!
 
I would even try the ssr using a white pad myself. Start with SSR1 if you got it though, that could even do the trick.
 