Yes, my girlfriend is close to having me committed for working this long on JUST the hood of my black 95' Miata. Here's what I found worked and didn't work.
3M medium cut compound is WAY too abrasive and caused major hazing. Scared me sh_tless after realizing what I had done, fortunately it came out, but took four more polishing runs with less abrasive chemicals.
DACP is horrible in my opinion. Sorry, I know it has a strong following, maybe I'm using it wrong but it is just plain hard to use, produces little results and dusts everywhere!
Menzurna FP is AWESOME on black. I used this more than anything. The IP was used as a base and hazed a bit. The FP took all the hazing out but I had to do each section maybe 3 times to get a nice shine. The more I kept repolishing with FP, the deeper the shine.
I thought I could intensify the deepness with Klasse AIO but to my suprise it caused hazing after Menzurna FP! I ended up skipping the AIO and going straight to the Klasse sealing glaze. Is AIO more abrasive than Menzurna FP?
After applying the sealing glaze I put a coat of S100 and didn't notice much difference. Will it be allright to apply more coats of sealing glaze over the S100? I want to put 4 or 5 coats of sealing glaze over a week's period.
Also, for the polishing I used only a speed of 2 or 3 with the FP, this allowed the working time to dramatically increase. Otherwise on speed 6 it would dry in under a minute and would be very hard to remove. Do you guys polish on speed 2 or 3?
Long post, sorry but I think I learned quite a bit. Any obsevations/comments are appreciated!
3M medium cut compound is WAY too abrasive and caused major hazing. Scared me sh_tless after realizing what I had done, fortunately it came out, but took four more polishing runs with less abrasive chemicals.
DACP is horrible in my opinion. Sorry, I know it has a strong following, maybe I'm using it wrong but it is just plain hard to use, produces little results and dusts everywhere!
Menzurna FP is AWESOME on black. I used this more than anything. The IP was used as a base and hazed a bit. The FP took all the hazing out but I had to do each section maybe 3 times to get a nice shine. The more I kept repolishing with FP, the deeper the shine.
I thought I could intensify the deepness with Klasse AIO but to my suprise it caused hazing after Menzurna FP! I ended up skipping the AIO and going straight to the Klasse sealing glaze. Is AIO more abrasive than Menzurna FP?
After applying the sealing glaze I put a coat of S100 and didn't notice much difference. Will it be allright to apply more coats of sealing glaze over the S100? I want to put 4 or 5 coats of sealing glaze over a week's period.
Also, for the polishing I used only a speed of 2 or 3 with the FP, this allowed the working time to dramatically increase. Otherwise on speed 6 it would dry in under a minute and would be very hard to remove. Do you guys polish on speed 2 or 3?
Long post, sorry but I think I learned quite a bit. Any obsevations/comments are appreciated!