Qship3000 said:All I can say is that after two Dawn apps, water was no longer beading; that's my sole criterion for removal, so perhaps I'm wrong about removal a la Dawn. After two rounds of clay plus the polish, I suspect all was gone.
Yeah, the polish'll take care of it anyhow. KSG can be weird about beading, you can't necessarilly use that as a measure of it...no biggie anyhow but if you ever get your polishing pads gumming up from KSG try using the rubbing alcohol.
OutlawTitan- I don't doubt that your KSG lasted that long. FWIW, I can always *feel* a healthy coat of SG, it has a "plastic" feel that's quite different from how paint feels with other LPS or when bare. Now that I'm putting FK 425 on the SG, it goes from feeling like plastic (the SG) to feeling like it has FK 425 on it. And when I had some areas repainted it was easy to tell the difference between those (either when bare or treated with Meg's #5 or 3M IHG) and the panels with KSG on them.