just got through a 3hr polishing session for my car... no... the car looked great after the detailing session... it was my 8" LC pad that had the problem... The foam pad delaminated from the velcro backing plate... was this expected if you continuously (well, not really continuous since i have to take 5 min break bet. panels) use the LC pad with a DW443.. i was not using it at speed#5 all the time... per panel, i think i dwell on the #5 setting for about 5mins per panel...
i complained to the local distributor here and he said to take some photos and he'll try to send it to the US, but it was a "long-shot".
for delaminated pads... can we glue back the velcro to the foam pad? if yes, what kind of glue can I use... thanks!
i complained to the local distributor here and he said to take some photos and he'll try to send it to the US, but it was a "long-shot".