What after SSR 2.5

Krisek

New member
Hey Guys...



What should I use after Orange Lake Pad and SSR 2.5

White Pad SFX ? + SSR 2 will be ok ?



If not what Meguiars ( available locally ) product I should use for final step .. before wax ..



Thank You
 
White or Blue/Black LC pad(if paint is on the soft side).



Im not familiar with SSRs but use the least aggressive one you have, maybe SSR 1.



Megs 80 or 205 would work great.
 
I find that SSR2.5 finishes down pretty well, so you shouldn't have any trouble on a light colored car, anyway. It does have some fillers or something in it, however. I don't know that SSR2 really finishes down any better, so SSR1 if you have it, or you can try the consumer version of 205...what is that, SwirlX? IMO 80 isn't going to be much different than SSR2.5.
 
XMT 1 (as long as its the least aggressive, Im not familiar with that either) will work. Or SSR 2 with white.



Sometimes you just need to try this stuff out and see for yourself, theres no definitive answer.



I would drop the EXP and just do a layer or 2 of fuzion.
 
SSR 2 orange, or SSR 2.5 orange if needed

XMT #1 white sonus SFX

Fuzion x2



that is how I would start

but you will prob need to play around and find what works for you
 