diff. kind of sandwiching - Meg. No. 3 w/ PC on top of Zaino ?

s2skimon

New member
I'm thinking of trying this and wanted to know if anyone else tried this with successful results ?



********

PC work -3M SMR, &/or FCC..(only if needed. )

Zaino - z2.. a couple of coats

PC apply Meguiar's No. 3 machine Polish

PC finish off by "heating up" the entire job with my MF towel bonnet.

*************



I know many friends of mine have started to sandwich s100 or other carnuba's onto of Zaino's z2. I'm a PC fanatic and wanted to take this sandwiching a step further. After my zaino stage, I was thinking of using my PC w/ Megiuar's No. 3 Machine Polish on top of my zaino ? Then crack out my MF bonnet and "heat it up" for greater "bling bling" ?



Supposedly Meg's No. 3 is specifically made for PC's so I'm curious to see if it makes the finish even "wetter" looking.



Has anyone else tried this ?



Your input is greatly appreciated



Thanks for your time
 
The only thing you are going to accomplish with the machine polish is taking OFF the zaino underneath.



edit: it might take off the Zaino, the #3 is supposedly non abrasive, but it might have solvents that will harm the zaino (plus it is pretty oily and will attract dust). I would stick with something safer like S100 or a pure carnuaba wax.
 
AHhh.. I seee..



so then let's remove the meguiar's PC no. 3 stage



and keep the MF Towel bonnet which would simply be heating up the Z2. Think that'll improve it ?
 
No, you'll probably just make swirls. The zaino cures chemically, no external heat is necessary or recommended. after the recommended 24hrs, it is fully cured and ready to go.
 