Hi, im still fighting micro swirling under halogen lighting. Ive worked #80 every which way but loose and still getting slight micro marring. My definition of micro marring is swirl scratching about 1/16in , that can only be seen a few inches away but there not as dense as the hazing after #83, just smaller and more sparse. The best thing ive been able to do is use #80 on the black Sonus finishing pad @ speed 6 and working it dry, and I mean dry to where there is hardly anything to wipe off. Ive read about working it till it changes color or leave it with the wet egde and or let it sit and cure 10 - 15 mins. What is this indicating about my paint? #80/finishing pad @ spd 6 working till dry?? PS by dry do we mean literally till there is absolutely no filming left at all? Some times I think we are all using the same words but describing different things. Thx